Luminescent properties of complexly substituted oxides Ме2Ln8 (XO4)6O2 (Me=Sr, Ca; Ln=La, Gd, Eu; X= Si, P)
In the current work it is established that the maximum intensity of a luminescence of crystalline phosphors with structure silicate-apatite of general formulae: Ca2Eu8Si6(1-x)P6xO26, Sr2Gd7.2Eu0.8Si6(1-x)P6xO26 and Ca2La8(1-x)Eu8xSi6O26 is reached at concentration of europium equal 0,15. The maximum...
Uloženo v:
| Vydáno v: | Chimica Techno Acta Ročník 1; číslo 1; s. 26 - 32 |
|---|---|
| Hlavní autoři: | , |
| Médium: | Journal Article |
| Jazyk: | angličtina japonština |
| Vydáno: |
Ural Federal University
30.06.2014
|
| Témata: | |
| ISSN: | 2411-1414 |
| On-line přístup: | Získat plný text |
| Tagy: |
Přidat tag
Žádné tagy, Buďte první, kdo vytvoří štítek k tomuto záznamu!
|
| Shrnutí: | In the current work it is established that the maximum intensity of a luminescence of crystalline phosphors with structure silicate-apatite of general formulae: Ca2Eu8Si6(1-x)P6xO26, Sr2Gd7.2Eu0.8Si6(1-x)P6xO26 and Ca2La8(1-x)Eu8xSi6O26 is reached at concentration of europium equal 0,15. The maximum intensity of a luminescence of these substances, at replacement in an anion sublattice of tetrahedrons [SiO4]4- on tetrahedrons [PO4]3- takes place at concentration of phosphorus 0,05. |
|---|---|
| ISSN: | 2411-1414 |