Luminescent properties of complexly substituted oxides Ме2Ln8 (XO4)6O2 (Me=Sr, Ca; Ln=La, Gd, Eu; X= Si, P)

In the current work it is established that the maximum intensity of a luminescence of crystalline phosphors with structure silicate-apatite of general formulae: Ca2Eu8Si6(1-x)P6xO26, Sr2Gd7.2Eu0.8Si6(1-x)P6xO26 and Ca2La8(1-x)Eu8xSi6O26 is reached at concentration of europium equal 0,15. The maximum...

Full description

Saved in:
Bibliographic Details
Published in:Chimica Techno Acta Vol. 1; no. 1; pp. 26 - 32
Main Authors: A. A. Vasin, M. G. Zuev
Format: Journal Article
Language:English
Japanese
Published: Ural Federal University 30.06.2014
Subjects:
ISSN:2411-1414
Online Access:Get full text
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:In the current work it is established that the maximum intensity of a luminescence of crystalline phosphors with structure silicate-apatite of general formulae: Ca2Eu8Si6(1-x)P6xO26, Sr2Gd7.2Eu0.8Si6(1-x)P6xO26 and Ca2La8(1-x)Eu8xSi6O26 is reached at concentration of europium equal 0,15. The maximum intensity of a luminescence of these substances, at replacement in an anion sublattice of tetrahedrons [SiO4]4- on tetrahedrons [PO4]3- takes place at concentration of phosphorus 0,05.