Surface tension and density of copper–Zirconium alloys in contact with fluoride refractories
The surface tension and density of copper–zirconium alloys were measured over a wide range of zirconium concentration (from 7.182 to 74.0 at.%) at temperatures between 1000 and 1250∘C by the “large drop” method in cups made on calcium fluoride. The surface tension and density polytherms are straight...