Durability of bonded FRP-to-steel jointsEffects of moisture, de-icing salt solution, temperature and FRP type
This paper investigates the effects of environmental ageing on the mechanical response of adhesively bonded double-lap shear joints made of steel and CFRP or GFRP adherents. One hundred and ninety-two specimens, 84 joints and 108 material coupons, were aged for up to three years in various environme...
Saved in:
| Published in: | Composites. Part B, Engineering Vol. 119; p. 153 |
|---|---|
| Main Authors: | , , |
| Format: | Journal Article |
| Language: | English |
| Published: |
15.06.2017
|
| Subjects: | |
| ISSN: | 1359-8368 |
| Online Access: | Get full text |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Abstract | This paper investigates the effects of environmental ageing on the mechanical response of adhesively bonded double-lap shear joints made of steel and CFRP or GFRP adherents. One hundred and ninety-two specimens, 84 joints and 108 material coupons, were aged for up to three years in various environments including (i) immersion in distilled water at 20 °C and 45 °C, (ii) immersion in de-icing salt solution at 20 °C and 45 °C and (iii) exposure to 95% relative humidity at 45 °C. In general, immersion at 45 °C resulted in noticeably greater strength reductions at both material and joint level. While the strength and stiffness of the joints made of GFRP material underwent significant reductions, the CFRP/steel joints were affected to a considerably smaller degree. FE simulations showed the impact of the permeability of FRP adherents and moisture distribution at the FRP/adhesive interface on the integrity and strength of the joints. The joint-level results are compared with the most relevant durability data in the literature. |
|---|---|
| AbstractList | This paper investigates the effects of environmental ageing on the mechanical response of adhesively bonded double-lap shear joints made of steel and CFRP or GFRP adherents. One hundred and ninety-two specimens, 84 joints and 108 material coupons, were aged for up to three years in various environments including (i) immersion in distilled water at 20 °C and 45 °C, (ii) immersion in de-icing salt solution at 20 °C and 45 °C and (iii) exposure to 95% relative humidity at 45 °C. In general, immersion at 45 °C resulted in noticeably greater strength reductions at both material and joint level. While the strength and stiffness of the joints made of GFRP material underwent significant reductions, the CFRP/steel joints were affected to a considerably smaller degree. FE simulations showed the impact of the permeability of FRP adherents and moisture distribution at the FRP/adhesive interface on the integrity and strength of the joints. The joint-level results are compared with the most relevant durability data in the literature. |
| Author | Heshmati, Mohsen Al-Emrani, Mohammad Haghani Dogaheh, Reza |
| Author_xml | – sequence: 1 givenname: Mohsen surname: Heshmati fullname: Heshmati, Mohsen organization: Structural Engineering – sequence: 2 givenname: Reza surname: Haghani Dogaheh fullname: Haghani Dogaheh, Reza organization: Structural Engineering – sequence: 3 givenname: Mohammad surname: Al-Emrani fullname: Al-Emrani, Mohammad organization: Structural Engineering |
| BackLink | https://research.chalmers.se/publication/248956$$DView record from Swedish Publication Index (Chalmers tekniska högskola) |
| BookMark | eNotj8lOwzAUAH0oEm3hH8y9Cd6SJkdUWkCqBGI5W16eqaskjmxHqH8PBU5zGY00CzQbwgAI3VBSUkLr22NpQj-G5DMkXTJC1yXhJRHtDM0pr9qi4XVziRYpHQkhouJsjvr7KSrtO59PODisw2DB4t3rS5FDkTJAh4_BDzltnQOT01nqg095irDCFgpv_PCJk-oyTqGbsg_DCmfoR4jqLGE1_PZwPo1whS6c6hJc_3OJPnbb981jsX9-eNrc7YtERW0LDURVLWstM7VoFBNaWMGaVnNwuiHw88IoZZy4tV5z0YJqnOCOA7NCiYryJXr766YvGCctx-h7FU8yKC8jJFDRHKQ5qK6HmGQC6YAYR4yRmtS1FBUTUteUSCUINdYxBrXl30kvcH8 |
| ContentType | Journal Article |
| DBID | ABBSD ADTPV AOWAS D8T F1S ZZAVC |
| DOI | 10.1016/j.compositesb.2017.03.049 |
| DatabaseName | SWEPUB Chalmers tekniska högskola full text SwePub SwePub Articles SWEPUB Freely available online SWEPUB Chalmers tekniska högskola SwePub Articles full text |
| DatabaseTitleList | |
| DeliveryMethod | fulltext_linktorsrc |
| Discipline | Engineering |
| ExternalDocumentID | oai_research_chalmers_se_fe0cf0cc_b066_4524_b610_a401cdf22e6d |
| GroupedDBID | --K --M .~1 0R~ 1B1 1~. 1~5 29F 4.4 457 4G. 5GY 5VS 6TJ 7-5 71M 8P~ AABXZ AAEDT AAEDW AAEPC AAIKJ AAKOC AALRI AAOAW AAQFI AAQXK AATTM AAXKI AAXUO AAYWO ABBSD ABFNM ABJNI ABMAC ABWVN ABXDB ABXRA ACDAQ ACGFS ACLOT ACNNM ACRLP ACRPL ADBBV ADEZE ADMUD ADNMO ADTPV ADTZH AEBSH AECPX AEIPS AEKER AEZYN AFJKZ AFRZQ AFTJW AGHFR AGQPQ AGUBO AGYEJ AHJVU AI. AIEXJ AIIUN AIKHN AITUG ALMA_UNASSIGNED_HOLDINGS AMRAJ ANKPU AOWAS APXCP ASPBG AVWKF AXJTR AZFZN BJAXD BKOJK BLXMC CS3 D8T EBS EFJIC EFKBS EFLBG EJD EO8 EO9 EP2 EP3 F1S FDB FEDTE FGOYB FIRID FNPLU FYGXN G-Q GBLVA HVGLF HZ~ IHE J1W JJJVA KOM M41 MAGPM MO0 N9A O-L O9- OAUVE OZT P-8 P-9 PC. Q38 R2- RNS ROL RPZ SDF SDG SDP SES SEW SPC SPCBC SSM SST SSZ T5K VH1 ZMT ZZAVC ~02 ~G- ~HD |
| ID | FETCH-LOGICAL-s146d-be0a5929d2c648a24b4d4289b3efb80e359211230f7b7349ea8f43f3e2d4a4513 |
| ISSN | 1359-8368 |
| IngestDate | Wed Nov 05 04:20:53 EST 2025 |
| IsDoiOpenAccess | true |
| IsOpenAccess | true |
| IsPeerReviewed | true |
| IsScholarly | true |
| Language | English |
| LinkModel | OpenURL |
| MergedId | FETCHMERGED-LOGICAL-s146d-be0a5929d2c648a24b4d4289b3efb80e359211230f7b7349ea8f43f3e2d4a4513 |
| OpenAccessLink | https://research.chalmers.se/publication/248956 |
| ParticipantIDs | swepub_primary_oai_research_chalmers_se_fe0cf0cc_b066_4524_b610_a401cdf22e6d |
| PublicationCentury | 2000 |
| PublicationDate | 2017-06-15 |
| PublicationDateYYYYMMDD | 2017-06-15 |
| PublicationDate_xml | – month: 06 year: 2017 text: 2017-06-15 day: 15 |
| PublicationDecade | 2010 |
| PublicationTitle | Composites. Part B, Engineering |
| PublicationYear | 2017 |
| SSID | ssj0004532 |
| Score | 2.5709586 |
| Snippet | This paper investigates the effects of environmental ageing on the mechanical response of adhesively bonded double-lap shear joints made of steel and CFRP or... |
| SourceID | swepub |
| SourceType | Open Access Repository |
| StartPage | 153 |
| SubjectTerms | Environmental degradation FRP-steel bonded joints Mechanical properties Polymer-matrix composites (PMCs) |
| Title | Durability of bonded FRP-to-steel jointsEffects of moisture, de-icing salt solution, temperature and FRP type |
| URI | https://research.chalmers.se/publication/248956 |
| Volume | 119 |
| hasFullText | 1 |
| inHoldings | 1 |
| isFullTextHit | |
| isPrint | |
| journalDatabaseRights | – providerCode: PRVESC databaseName: Elsevier SD Freedom Collection Journals 2021 issn: 1359-8368 databaseCode: AIEXJ dateStart: 19960101 customDbUrl: isFulltext: true dateEnd: 99991231 titleUrlDefault: https://www.sciencedirect.com omitProxy: false ssIdentifier: ssj0004532 providerName: Elsevier |
| link | http://cvtisr.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwtV1bi9NAFB5qV0QfxCveGcG3biBNJrfHql1WWZZFVuhbmMuZptIkS5Mui7_Gn-qZmbSJN1DUl1DSdkjyfZx8c-bMdwh5FUcQRwnnnkwBPCa08tJIC49Fmc8YCFQkFumT5PQ0XSyys9Hoy24vzOU6qar06iq7-K9Q4zkE22yd_QO494PiCfyMoOMRYcfjbwH_drtx3tt27VzUJsU9Ofpw5rW1h5CCcYtYVW0z7ys5yhrB3rpstALPLLYvJw1ft5PdpZpvjItVZ8FslxxwTJvBHepbE15MGRhOv1GcbtrJaxtse9PDPvfaFEYs24RsXTT9jrRjvix4tUJpv-QFFI4Dn_dvj9nam5cb14nK_JOXJVfD3MXUFtq53ZtduA1NEjJ0jXX28biLoS6iTp2X8A-R3iUdPhmguvsSplAvsZa1zgX1J0banYNSkcvCtqdp8gZyDb7UvpS5QP2VsyhguUBVmXOce0qlgwBidY0cBEmUpWNyMHs3X7wfONLbJnj7O7lBXvY1hL-4uO9saa2UOb9DbndzEDpz3LlLRlDdI7cGIN0nZc8iWmvqWESHLKLfsMj8aMeiQ7rjEDUcojsOHdIBgygyyIxHDYMekI9H8_M3x17XmcNr8M2qPAE-j1BYq0DGLOUBE0zhPDYTIWiR-oAPI0AhH_o6EUnIMuCpZqEOIVCMs2gaPiTjqq7gEaEYDGQSqWmcAmeQyoz5UsUyiyBjGlT2mJy4Z5VfOPuV_K9wfPJvh3tKbva8fkbG7WYLz8l1edmums2LjitfATiKnlE |
| linkProvider | Elsevier |
| openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=Durability+of+bonded+FRP-to-steel+jointsEffects+of+moisture%2C+de-icing+salt+solution%2C+temperature+and+FRP+type&rft.jtitle=Composites.+Part+B%2C+Engineering&rft.au=Heshmati%2C+Mohsen&rft.au=Haghani+Dogaheh%2C+Reza&rft.au=Al-Emrani%2C+Mohammad&rft.date=2017-06-15&rft.issn=1359-8368&rft.volume=119&rft.spage=153&rft_id=info:doi/10.1016%2Fj.compositesb.2017.03.049&rft.externalDocID=oai_research_chalmers_se_fe0cf0cc_b066_4524_b610_a401cdf22e6d |
| thumbnail_l | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=1359-8368&client=summon |
| thumbnail_m | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=1359-8368&client=summon |
| thumbnail_s | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=1359-8368&client=summon |